N2 - Advances in materials for power plants include not only new materials with higher-temperature capabilities, but also the use of current materials at increasingly higher temperatures. This latter activity builds on extensive experience of the performance of the various alloys, and provides a basis for identifying changes in alloy behavior with increasing temperature as well as understanding the factors that ultimately determine the maximum use temperatures of the different alloy classes. This paper presents results from an effort to model the exfoliation processes of steam-side oxide scales in a manner that describes as accurately as possible the evolution of strains in oxides growing inside small-diameter tubes subjected to large thermal gradients and to thermal transients typical of normal steam boiler operation. One way of portraying the results of such calculations is by plotting the evolving strains in a given oxide scale on an 'Exfoliation Diagram' (of the type pioneered by Manning et al. of the British Central Electricity Research Laboratory) to determine the earliest time at which the trajectory of these strains intersects a criterion for scale failure. Understanding of how such 'strain trajectories' differ among different alloys and are affected by the major variables associated with boiler operation has the potential to suggest boiler operating strategies to manage scale exfoliation, as well as to highlight the mode of scale failure and the limitations of each alloy. Preliminary results are presented of the strain trajectories calculated for alloys T22, T91, and TP347 subjected to the conditions experienced by superheaters under assumed boiler operating scenarios. For all three alloys the earliest predicted scale failures were associated with the increased strains developed during a boiler shut-down event; indeed, in the cases considered it appeared unlikely that scale failure would occur in any practically meaningful time due to strains accumulated during operation in a load-following mode in the absence of a shut down. The accuracy of the algorithms used for the kinetics of oxide growth appeared to be a very important consideration, especially for alloy TP347 for which large effects on oxide growth rate are known to occur with changes in alloy grain size and surface cold work.
AB - Advances in materials for power plants include not only new materials with higher-temperature capabilities, but also the use of current materials at increasingly higher temperatures. This latter activity builds on extensive experience of the performance of the various alloys, and provides a basis for identifying changes in alloy behavior with increasing temperature as well as understanding the factors that ultimately determine the maximum use temperatures of the different alloy classes. This paper presents results from an effort to model the exfoliation processes of steam-side oxide scales in a manner that describes as accurately as possible the evolution of strains in oxides growing inside small-diameter tubes subjected to large thermal gradients and to thermal transients typical of normal steam boiler operation. One way of portraying the results of such calculations is by plotting the evolving strains in a given oxide scale on an 'Exfoliation Diagram' (of the type pioneered by Manning et al. of the British Central Electricity Research Laboratory) to determine the earliest time at which the trajectory of these strains intersects a criterion for scale failure. Understanding of how such 'strain trajectories' differ among different alloys and are affected by the major variables associated with boiler operation has the potential to suggest boiler operating strategies to manage scale exfoliation, as well as to highlight the mode of scale failure and the limitations of each alloy. Preliminary results are presented of the strain trajectories calculated for alloys T22, T91, and TP347 subjected to the conditions experienced by superheaters under assumed boiler operating scenarios. For all three alloys the earliest predicted scale failures were associated with the increased strains developed during a boiler shut-down event; indeed, in the cases considered it appeared unlikely that scale failure would occur in any practically meaningful time due to strains accumulated during operation in a load-following mode in the absence of a shut down. The accuracy of the algorithms used for the kinetics of oxide growth appeared to be a very important consideration, especially for alloy TP347 for which large effects on oxide growth rate are known to occur with changes in alloy grain size and surface cold work.
UR - http://www.scopus.com/inward/record.url?scp=79958288084&partnerID=8YFLogxK
M3 - Conference contribution
AN - SCOPUS:79958288084
SN - 9781615037247
T3 - Advances in Materials Technology for Fossil Power Plants - Proceedings from the 6th International Conference
SP - 213
EP - 242
BT - Advances in Materials Technology for Fossil Power Plants - Proceedings from the 6th International Conference