Original language | English |
---|---|
Pages (from-to) | 2866-2868 |
Number of pages | 3 |
Journal | Metallurgical Transactions A |
Volume | 20 |
Issue number | 12 |
DOIs | |
State | Published - Dec 1989 |
Externally published | Yes |
Solidification of the nickel-base superalloy 718: A phase diagram approach
B. Radhakrishnan, R. G. Thompson
Research output: Contribution to journal › Article › peer-review
53
Scopus
citations