High-temperature compressive creep tests of U3Si2 with spark plasma sintering: Experiments and finite element modeling

Research output: Contribution to journalArticlepeer-review

6 Scopus citations

Fingerprint

Dive into the research topics of 'High-temperature compressive creep tests of U3Si2 with spark plasma sintering: Experiments and finite element modeling'. Together they form a unique fingerprint.