Emergence of micro-galvanic corrosion in plastically deformed austenitic stainless steels

Xin Chen, Maxim Gussev, Magdalena Balonis, Mathieu Bauchy, Gaurav Sant

Research output: Contribution to journalArticlepeer-review

51 Scopus citations

Fingerprint

Dive into the research topics of 'Emergence of micro-galvanic corrosion in plastically deformed austenitic stainless steels'. Together they form a unique fingerprint.

Engineering

Material Science