Abstract
Iron is a key ductility-limiting impurity in secondary Al-Si alloys that is responsible for impeding their widespread use in structural applications. An Al-7Si-0.3 Mg alloy with 0.5% Cu and 1% Fe (all in wt.%) was fabricated via laser powder-bed fusion to explore new microstructure engineering pathways with this processing route. While highly refined β-Al5FeSi intermetallic particles rendered the alloy high strength (yield strength of ∼220-250 MPa and ultimate tensile strength of ∼450 MPa), its unusually high strain-hardening rate also led to a moderate ductility of ∼4% in the as-printed state. The high strain-hardening rate was attributed to the development of internal back stresses around high-aspect-ratio, non-shearable β-Al5FeSi particles, which produced a large kinematic contribution to strain hardening. Two heat treatment based microstructure control strategies were applied to manage the strain-hardening rate, thereby improving alloy ductility. Direct aging at 150°C for 15 h produced numerous shearable βˈˈ-MgSi precipitates in α-Al matrix with no effect on β-Al5FeSi characteristics, which doubled the ductility relative to as-fabricated state while retaining comparable strength. Alternatively, a short solutionizing treatment at 530°C led to fragmentation of β-Al5FeSi, making them less prone to internal stress development, and subsequent aging produced shearable βˈˈ-MgSi precipitates with the microstructure leading to a high yield strength of ∼220 MPa and a ductility value of ∼20%. The findings of this study offer insights into the feasibility of upcycling secondary Al alloys for structural applications using additive manufacturing and, more broadly, into the ways of controlling the strain-hardening behavior of Al alloys for improved strength and ductility.
| Original language | English |
|---|---|
| Article number | 151095 |
| Journal | Materials Science and Engineering: A |
| Volume | 977 |
| DOIs | |
| State | Published - Dec 2026 |
Funding
The research was sponsored by the Light Metals Core Program (LMCP) under the Transportation Technologies Office, Office of Critical Minerals and Energy Innovation, US Department of Energy. The authors thank Sarah Grahams, Brian Long, Caitlin Duggan, Dana McClurg, Bryce Abbot, Michael Thompson, James Burns and Kelsey Epps for technical assistance with metallography, heat treatments, and mechanical testing. Notice: This manuscript has been authored by UT-Battelle, LLC under Contract No. DE-AC05-00OR22725 with the U.S. Department of Energy. The United States Government retains and the publisher, by accepting the article for publication, acknowledges that the United States Government retains a non-exclusive, paid-up, irrevocable, world-wide license to publish or reproduce the published form of this manuscript, or allow others to do so, for United States Government purposes. The Department of Energy will provide public access to these results of federally sponsored research in accordance with the DOE Public Access Plan ( http://energy.gov/downloads/doe-public-access-plan ).
Keywords
- Additive manufacturing
- Ductility
- Microstructure
- Secondary Al alloys
- Strain hardening
- Strength
Fingerprint