Direction-dependent receptances for anisotropic nickel superalloy

  • Andrew Honeycutt
  • , Mike Glavicic
  • , Tony L. Schmitz

Research output: Chapter in Book/Report/Conference proceedingConference contributionpeer-review

Original languageEnglish
Title of host publicationProceedings - 33rd ASPE Annual Meeting
PublisherAmerican Society for Precision Engineering, ASPE
Pages283-287
Number of pages5
ISBN (Electronic)9781887706773
StatePublished - 2018
Externally publishedYes
Event33rd Annual Meeting of the American Society for Precision Engineering, ASPE 2018 - Las Vegas, United States
Duration: Nov 4 2018Nov 9 2018

Publication series

NameProceedings - 33rd ASPE Annual Meeting

Conference

Conference33rd Annual Meeting of the American Society for Precision Engineering, ASPE 2018
Country/TerritoryUnited States
CityLas Vegas
Period11/4/1811/9/18

Funding

The authors gratefully acknowledge financial support from MAI BA-21 (USAF contract number FA8650-17-2-5246).

Cite this